The work presents an analysis of the recycling potential of thin-walled aluminum within the framework of a circular economy (CE). The analysis focused on the undersized fraction derived from the processing of municipal waste in Mechanical Biological Treatment (MBT) facilities. After the mechanical processing of the incoming waste, it passes through screens, where the so-called undersized fraction is separated, the composition of which varies over time due to the seasonality of municipal waste and the origin of the waste. As part of the conducted work, an attempt was made to determine the variability over time; the studies lasted 12 months and assessed the possibility of recovering thin-walled aluminum from the municipal waste stream. During the research, a series of trial melts were performed using modified fluxes based on cryolite with the addition of NaCl. The work was carried out using a laboratory induction crucible furnace
The growing demand for manufacturing steel components in the manufacturing industry is forcing the rapid development of metal welding technology. One of the modern welding techniques is the joining of components using laser welding, where the material is joined using a focused laser beam. This method makes it possible to achieve high process efficiency, while maintaining cleanliness in the welding area and high-quality welded joints. In the conducted research, the laser beam welding method (method 52) was compared with the conventional TIG welding method (method 141), to compare the welding time, the effect of temperature in the HAZ after welding and the quality of the resulting welds.
This publication presents the results of dielectric strength tests conducted on selected materials. The methodology for sample fabrication is described, utilizing two different spatial printing technologies. The tested samples were manufactured from four materials with varying properties: PLA, ABS, PA12, and a recycled material (e-PLA). Significant differences in dielectric strength were observed, both among the individual materials and between the applied manufacturing technologies. It was determined that samples made of PA12, produced using laser sintering (SLS) technology, exhibited the highest dielectric strength. The objective of the study was to evaluate the feasibility of producing insulating components for power transmission and distribution lines through dielectric strength testing. Preliminary results indicate that, with the appropriate technology and material selection, this manufacturing approach may be a viable alternative for such applications.
The study presents a series of experiments focused on cleaning the active surface of a conventional grinding wheel using two methods of supplying the cooling and lubricating fluid with minimum consumption: MQL (Minimum Quantity Lubrication) and the flood method WET (wet machining) with an oil–water emulsion, during the process of plunge surface grinding in both up- and down-grinding modes. The tests were carried out on steel grade 1.4034 with a hardness of 55 HRC. A special design solution of the 38A60KV8 grinding wheel (Norton Poland) was proposed, which enabled observation of the behavior and deposition of contaminants on the sample surface. A methodology was developed for collecting contaminants on the surface of the ground material. The contaminants from the active surface of the grinding wheel (CPS) were weighed. The obtained results made it possible to assess the effectiveness of the investigated methods of supplying the cooling and lubricating fluid (PCS). In particular, it was found that perpendicular delivery of PCS supports the lubrication of the ground surface, positively affects the cutting forces by reducing friction, and consequently lowers the temperature in the machining zone, which in turn contributes to achieving a more favorable distribution of compressive stresses in the surface layer.”
This paper presents an analysis of the anisotropy of mechanical properties of the investigated sheets based on the results of static tensile testing and HV hardness measurements. The objective of the study was to evaluate variations in mechanical properties in three key areas along the coil length. In addition, an analysis across the sheet width was performed. It was found, among other things, that there are clear differences in hardness between the beginning, middle, and end areas of the coil. The differences in hardness ranged from approximately 2.3 to as much as 12.9 units, with higher values observed for hot-rolled sheets. Differences in hardness between the edge and the center of the sheet were also observed in all three zones. The largest differences in yield strength and tensile strength values, regardless of steel grade, were obtained across the sheet width at the beginning or end of the coil. Based on the analysis of the obtained results, the level of anisotropy of the mechanical properties of the sheets was determined for the individual dimensions and steel grades. The results demonstrated that anisotropy is more pronounced across the sheet width than along the coil length. It was also shown that hot-rolled sheets exhibit higher anisotropy compared to cold-rolled sheets. The obtained results provided the basis for developing an innovative tension-straightening technology for sheets uncoiled from coils and formed into flat sheets.
Praca została dofinansowana ze środków Narodowego Centrum Badań i Rozwoju (NCBiR), nr grantu POIR.01.01.01-00-0477/18.
This study numerically investigates the ballistic behavior of stitched and unstitched carbon fiber-reinforced composite plates using the finite element method. Simulations were performed under high-velocity impact conditions using ANSYS Workbench, with a projectile velocity of 350 m/s and appropriate boundary constraints. The results reveal that stitched composites exhibit higher values in internal (4.90 × 10⁵ J) and contact energy components (5.56 × 10⁵ J) compared to unstitched composites (4.22 × 10⁵ J and 1.19 × 10⁵ J, respectively). This indicates that stitching enhances load transfer at the fiber–matrix interfaces and facilitates more effective distribution of the absorbed energy through structural deformation. Although unstitched composites show slightly higher total energy absorption (5.74 × 10⁶ J) than stitched ones (5.52 × 10⁶ J), a significant portion of this energy remains in the form of kinetic energy (5.32 × 10⁶ J vs. 5.27 × 10⁶ J), contributing less to structural absorption. Consequently, while unstitched composites demonstrate a more brittle behavior, stitched composites dissipate energy more effectively through internal deformation and contact mechanisms, resulting in superior ballistic performance. The findings provide valuable insights for the design of impact-resistant composite structures in defense and aerospace applications.
The paper characterizes the castings of bottom plates used in chamber furnaces for heat treatment. Their typical structures and damages that occur in these castings during operation are presented. Bottom plates usually have a rectangular shape adapted in dimensions to the hearth of chamber furnaces. They consist of one or several segments, depending on the length of the furnace chamber. They are cast in sand molds. Plate castings are commonly made of high-chromium heat-resistant cast steel or heat-resistant chromium-nickel cast steel melted in crucible induction furnaces. Appropriate grades of cast steel and operating conditions of plates in which the use of individual alloys is recommended are indicated. Material, design and casting factors that plate designers take into account to ensure appropriate functional properties of castings are also discussed. This work is a review, its main purpose being to provide a summary of the current state of knowledge and the most important issues related to the design, manufacture, and operation of bottom plates.
This paper presents a comparative analysis of tool steels applied in cutting forms for paper cutlery manufacturing. The study was initiated after the original tool material, martensitic stainless steel 440C (HRC 56–58), demonstrated insufficient wear resistance plus is easily damaged, broken and required frequent sharpening. Four alternative Uddeholm steels—Sverker 21, Sleipner, Unimax, and Tyrax ESR—were tested under identical production conditions. Two of them (Unimax and Sverker 21) were coated with Duplex-Tigral PVD coating. The objective was to evaluate wear mechanisms, lifetime, and maintenance needs during stamping of 1000 gsm laminated cupstock paper. Tool wear was assessed using visual inspection and 3D scanning after approximately 500,000 cutting cycles. The results revealed that coated Unimax and Sleipner steels offered improved durability and reduced adhesive wear compared to the baseline. Average sharpening intervals increased from 0.5 to nearly 1 million cycles, although below the designed 2 million. Premature wear and paper residue accumulation caused additional downtime of up to 10 days per sharpening. The study highlights that an optimal combination of tool steel grade and PVD coating can significantly reduce maintenance frequency and operational costs in automated paper cutlery production.
The main purpose of this paper is the presentation of possibilities of using elements of SPC in the analysis of selected parameters of product manufactured in an industrial enterprise producing metal components and the analysis of causes of parameter deviations in control charts and their correction possibilities. As a tested product metal element used in automotive industry was chosen. Five parameters of the manufactured product were tested. During production process every hour 6-element samples were taken. In the analysis 30 samples were considered. Statistical analysis of selected parameters was done. According to this analysis the causes of parameter deviations in control charts were identified and their correction possibilities were proposed. As main causes of problems three main types of elements were identified: machines, tools and people.
Traceability is essential in modern manufacturing to ensure product quality, safety, and compliance throughout production and operation. In sectors such as automotive and aerospace, reliable component identification supports process control, maintenance, and failure analysis. Conventional marking methods often fail under difficult thermal conditions, creating demand for more robust solutions. This study evaluates the durability and readability of laser-engraved codes on aluminum components under conditions representative of industrial environments. Codes were engraved on surfaces with varying geometries, textures, and temperature, then exposed to elevated temperatures treatments. Their performance was assessed using industrial and mobile scanning devices to determine suitability for traceability systems in demanding manufacturing processes.
Traceability Solutions in Foundry Processes: Pilot Study of Laser and Camera-Based Product Identification Systems
- 1. Lodz University of Technology
Abstrakt
Traceability is essential in modern manufacturing to ensure product quality, safety, and compliance throughout production and operation. In sectors such as automotive and aerospace, reliable component identification supports process control, maintenance, and failure analysis. Conventional marking methods often fail under difficult thermal conditions, creating demand for more robust solutions. This study evaluates the durability and readability of laser-engraved codes on aluminum components under conditions representative of industrial environments. Codes were engraved on surfaces with varying geometries, textures, and temperature, then exposed to elevated temperatures treatments. Their performance was assessed using industrial and mobile scanning devices to determine suitability for traceability systems in demanding manufacturing processes.
Introduction
Traceability refers to the capability to record and represent all processes associated with a specific product [1]. This term refers both to internal traceability, i.e., tracking and tracing products and processes within a single stakeholder’s operations, and inter-supply chain traceability. As an enabling technology, traceability supports numerous applications, such as improving the accuracy of quality-related recalls [2]. In the automotive industry, one of the key challenges is the existence of multiple fragmented traceability systems and diverse data formats, which hinder efficient product tracking across the supply chain. Standardizing these systems and integrating identification processes can significantly improve operations, including the recall of defective batches [3]. Tracking and automatic identification systems are becoming essential for analyzing business processes, reducing losses, and improving product quality. Implementing traceability enables automated collection and processing of production data. After system deployment, production efficiency increases, demonstrating that such solutions can deliver not only financial benefits but also long-term improvements in monitoring and managing production flow. Similar cases have been observed in the foundry industry, which is particularly challenging due to process characteristics involving high temperatures and the need for subsequent external machining of components [4]. Traceability data are valuable beyond crisis management, such as recalls or proof of compliance. The need for traceability spans a wide range of industries, from foundries to aerospace. Modern automated systems generate extensive data that enable real-time monitoring of components, production performance, and product quality. Incorporating traceability into process design supports efficiency, innovation, and long-term competitiveness [5].
The casting process involves melting a metal alloy and pouring it into a mold, where it solidifies into the desired shape. It typically requires maintaining high temperatures – often several hundred degrees Celsius above the alloy’s melting point – to ensure proper fluidity and filling of the mold. After solidification, cast parts usually undergo surface treatment and machining to remove imperfections, improve dimensional accuracy, and enhance surface quality. The process is valued for producing complex shapes efficiently, but careful control of temperature, cooling rate, and post-processing is essential to achieve good mechanical and aesthetic properties [6]. A constant high temperature (200°C) is often required in foundry processes because it affects the stability of the Al alloy [7]. In this regard, the process of product marking and the implementation of full traceability in the foundry process is particularly challenging when attempting to identify the product from the moment of casting to the finished product.
There are many marking methods, such as laser engraving, inkjet printing, dot peen marking, electrochemical etching, and the use of labels with printed codes. The choice of the appropriate technology depends on the purpose, budget, and type of material to be marked, taking into account the capabilities and limitations of each method. The criteria for selecting a technology can be based on the evaluation of factors such as flexibility, equipment cost, marking cost, marking speed, contrast (code visibility), stress load on the material, recognition method, and the complexity of system integration. A method with high potential for implementation in the casting process is laser marking. The mark is durable, the method allows for rapid marking, and it maintains high code quality parameters, such as contrast, even after heat treatment [8].
Laser marking is a precise, non-contact technique that employs a concentrated laser beam to alter the material’s surface layer, producing a permanent contrast for encoding alphanumeric or graphic information. In aluminum alloys, the laser interacts with the metal surface through localized melting, oxidation, or ablation, depending on parameters such as wavelength, pulse duration, and energy density [9], [10].
Laser marking depends strongly on process parameters, specifically laser power, scanning speed, frequency, pulse duration, and raster step. For anodized aluminum, the highest marking contrast was achieved at a scanning speed of 25 mm/s and a raster step of 25 µm. Increasing laser power and frequency further enhanced the contrast but also led to higher surface roughness. Optimal conditions were obtained at a frequency of 2 kHz and maximum laser power, producing stable, high-contrast markings with minimal roughness. These parameter relationships allow for precise control of marking quality and durability on aluminum surfaces [11].
Machine-readable codes are symbols or patterns that can be automatically interpreted by devices such as scanners or cameras, enabling efficient data capture without manual input. These codes include several types used in product tracking and serialization systems. One-dimensional (1D) codes, such as traditional barcodes, are simple to implement and inexpensive to print, but they have limited data capacity. Two-dimensional (2D) codes, like QR and DataMatrix, allow much larger amounts of information to be stored in a small space, which is advantageous for industries requiring detailed identification. This type of codes is widely applied in different industries due to growing needs for traceability and authentication. Compared to 1D codes, their implementation is more costly but provides greater security and flexibility in data management [12]. For metal marking applications, it is essential to consider machine-readable codes, such as DataMatrix, because they ensure the high efficiency required in production lines. These solutions are classified as simple marking methods, offering reliable and automated data capture without manual intervention [13].
Based on the analysis of literature and current traceability requirements, a study was conducted to evaluate the durability and readability of laser-engraved codes on aluminum components with varied geometries (flat, curved), surface textures (smooth, rough), and temperature conditions. The samples were subjected to heat treatment at 230°C for 8 hours and additionally verified under industrial conditions at 500°C.
Research Methodology
The aim of the study was to assess the durability and legibility of laser-engraved codes on aluminum components under conditions simulating industrial casting processes. Laser engraving was performed using an industrial laser on various aluminum surfaces characterized by different structures and geometries, including flat, curved, and roughened surfaces. The marking process utilized the DataMatrix method, implemented in multiple size variants: 3 × 3 mm, 4 × 4 mm, and 9 × 9 mm. This approach allowed for evaluating the influence of code dimensions on readability and durability under diverse material and geometric conditions. Additionally, markings were applied to two aluminum parts that had been preheated to 200°C prior to engraving, in order to evaluate the impact of substrate temperature on the quality and contrast of the markings. The initial code readings were conducted before the heat treatment using an industrial camera from a distance of 15–40 cm.
Subsequently, all three aluminum samples underwent heat treatment at 230°C for 8 hours to simulate prolonged exposure to thermal conditions typical of casting or operational processes. After the heat treatment, the codes were re-read using the camera of an iPhone 13 running iOS 18 (2025). Following the laboratory tests, the solution was also verified under real industrial conditions, including exposure to a heat treatment process at 500°C for 5 to 8 hours, followed by cooling to 90–100°C using coolant, and subsequent etching.
Results
Laser engraving was successfully applied to aluminum components with various surface characteristics, including flat, curved, glossy, and rough textures. All codes engraved on these surfaces were correctly read using an industrial camera from distances ranging between 15 cm and 40 cm. The markings remained legible regardless of surface geometry or initial substrate temperature, including samples preheated to 200°C prior to engraving. Data collected from the readability test is presented in Table 1.
The table summarizes the results of readability tests for DataMatrix codes marked on aluminum samples. It includes a Sample Photo showing the marked component, Sample Characteristics describing the shape, surface texture and finish (e.g., flat, glossy, rough), as well as additional conditions such as shadow presence and whether the sample was preheated before marking. The next columns specify the Data Matrix Size (e.g., 3×3 mm, 4×4 mm, 9×9 mm) and Camera Distance during the test. The final column, Code Readability Test (Camera-Based), records whether the camera successfully decoded the code; if the code was read without difficulty, the result is marked as “OK”. All codes were successfully read by the camera without any issues, regardless of the sample characteristics such as surface texture, shadow presence, or preheating conditions. This confirms that variations in these factors did not affect the readability of the DataMatrix markings.
Table 1. Laser-engraved code readability on aluminum surfaces
Next all three samples underwent heat treatment at 230°C for 8 hours. After this process, the codes were re-scanned using a simple iPhone 13 camera (iOS 18). In all cases, the markings remained intact and fully readable. The pictures of the engraved data matrix before and after heat treatment are presented in Table 2.
Table 2. Laser-engraved code readability on aluminum surfaces before and after heat treatment at 230°C for 8 hours.
After successful laboratory tests on aluminum samples, additional trials were carried out under real industrial conditions at a factory producing automotive components. These tests were performed directly on parts manufactured by the company to evaluate marking durability in a production environment. Components underwent a heat cycle at 500°C for 5–8 hours, followed by cooling to 90–100°C using coolant and subsequent etching. Even after these demanding procedures, all DataMatrix codes retained their integrity and were successfully read by mobile devices, confirming their reliability for traceability in the automotive industry.
Conclusions
The tests showed that laser marking provides durable and legible codes on aluminum components, even under challenging industrial conditions. The markings remained readable after exposure to high temperatures both in laboratory settings (230°C for 8 hours) and in industrial processes involving heating up to 500°C, cooling with liquid, and etching. Good results were also observed on parts that had already reached a temperature of 200°C before marking, indicating that the method works well even when components are preheated. These findings confirm that laser marking is a reliable solution for maintaining traceability of aluminum parts throughout various stages of production.